India's Largest Stockist and Supplier Of Nickel Alloys Since 2007

Hastelloy C276

Hastelloy C276 Quick Details
ASTM of Hastelloy C276 B574, B622, B366, B575, B564, B626, B619
Density 8.89 g/cm³
Melting Point 1325°C - 1370°C
Temprature Range 1.323 - 1.371°C
Specifications UNS N08825, WNR 2.4858, AFNOR NC19FeNb, EURONORM NiCr22Mo9Nb, OR ЭИ602, BS NA 21, JIS NCF 825, GOST ХН75МБТЮ,
Origin European, Japanese, American, Korean
Delivery Time
  • Malaysia : 6-8 Days
  • Italy: 25-30 Days

To Get Quote Within 4 Hours Click Here

 

Hastelloy C276 Specification

 

Table of Content

Alloy C276 Material Supplier in India Available in Various Forms, See Chemical Composition

Alloy C276 Chemical Composition
Grade Si Co P Mn Ni Cr S Fe Mo C
Hastelloy c276 0.08 max 2.50 max 0.04 max 1.00 max 50.99 min* 14.50 - 16.50 0.03 max 4.00 - 7.00 15.00 - 17.00 0.010 max

 

Hastelloy Alloy C276 Specification
Alloy 625 International Standards
UNS Number N10276
Standards ASTM B564, B622, B626, B366, B462, B574, B575, B619, B775
WNR Number 2.4819
Hastelloy Alloy C276 Material Specification
Alloy/Form ASTM ASME DIN
Plate, Sheet & Strip B-575 SB-575 17750
Rod & Bar B-574 SB-574 17752
Forgings B-564 SB-564 17754
Seamless Pipe & Tube B-622 SB-622 17551
Welded Pipe B-619 SB-619 -
Fittings B-366 SB-366 17744

Buy UNS N10276 Suitable To Work At Temperature Range 1.323 - 1.371°C, Refer Mechanical Properties

Alloy C276 Mechanical Properties
Property 21°C 200⁰C 100⁰C 300⁰C 300⁰C
Ultimate Tensile Strength for sheet 5 to ≤ 20 mm thick 700-950 - - - -
Ultimate Tensile Strength for sheet ≤ 5 mm thick 750-1000 - - - -
Ultimate Tensile Strength for bar ≤ 90 mm thick 700-950 - - - -
0.2% Yield Strength for sheet 5 to ≤ 20 mm thick - 255 255 170 200
0.2% Yield Strength for sheet ≤ 50 mm thick - 240 280 195 220
0.2% Yield Strength for bar ≤ 90 mm thick - 225 255 170 200
Charpy Impact V-notch indicidual value / J 67 (39 when welded) - - - -
Charpy Impact V-notch mean value / J 96 (56 when welded) - - - -
Elongation, % for sheet 5 to ≤ 20 mm thick 25 - - - -
Elongation, % for bar ≤ 90 mm thick 35 - - - -
Elongation, % for sheet ≤ 5 mm thick 30 - - - -
What is the cost of Hastelloy C276 in India?
For Most Updated Hastelloy C276 Price Click Here
Material Price In INR Price In USD
Hastelloy C276 ₹ 6000 - Per kg $ 75 - Per kg

Stockist Of European and Japanese Origin WNR 2.4819 in Mumbai With Density 8.89 g/cm³

Nickel C276 Equivalent
STANDARD UNS GOST OR JIS EN WERKSTOFF NR.
Hastelloy c276 N10276 ХН65МВУ ЭП760 NW 0276 NiMo16Cr15W 2.4819
Physical Properties of Nickel Alloy C276
Melting Range °F 2,415 - 2,500
°C 1,325 - 1,370
Density lb/in3 0.321
g/cm3 8.89
Specific Heat Btu•lb•°F 0.102
J/kg•°C 427
Shear Modulus 103 ksi 11.4
GPa 79
Young’s Modulus 103 ksi 29.8
GPa 205
Thermal Conductivity Btu•in./ft2•h°F 67.9
W/m•°C 9.8
Permeability at 200 oersted (15.9 kA/m) 1.0002
Poisson’s Ratio 0.307
Alloy C276 Size Range
Product form Size range from Size range to
Alloy C276 Pipe Fittings 0.5 in 8 in
Alloy C276 Pipe 0.5 in 8 in
Alloy C276 Flanges 0.5 in 8 in
Alloy C276 Tube 12 mm 260 mm
Which sectors use Alloy C276 Metal most frequently ?
WNR 2.4819 Applications

 

Offer Corrosion Resistance Inconel C276 Alloy With 197 HV Hardness At Lowest Possible Price
Nicrofer® 5716 Hardness
Form Typical ASTM Grain Size Hardness, HRBW
Plate 1 - 5 88
Sheet 3.5 - 6 88
Bar 1 - 5 86
Elevated Temperature Dynamic Modulus Properties of Haynes Alloy C276
Temp. Shear Modulus Young’s Modulus Poisson’s Ration
°F 103 ksi 103 ksi
70 11.81 31.30 0.33
100 11.75 31.18 0.33
200 11.57 30.77 0.33
300 11.40 30.35 0.33
400 11.23 29.92 0.33
500 11.05 29.42 0.33
Alloy C276 Average Tensile Data at Temperatures
Form Condition Test Temp °F (°C) YS 0.2% Ksi UTS Ksi Elon. in 2"(%)
Sheet, 0.094" (2.4mm) thick Heat-Treated
at 2050 °F (1121 °C)
Rapid Quenched
400 (204)
600 (316)
800 (427)
39.9
33.5
29.7
101.0
97.6
93.5
58
64
64
Plate 3/16 to 1" (4.8 to 25.4mm) thick Heat-Treated
at 2050 °F (1121 °C)
Rapid Quenched
400 (204)
600 (316)
800 (427)
1000(538)
38.2
34.1
32.7
32.8
98.9
94.3
91.5
87.2
61
66
60
59
Plate 1" (25.4mm) thick Heat-Treated
at 2050 °F (1121 °C)
Rapid Quenched
Room
600 (316)
800 (427)
52.9
36.2
30.5
113.9
96.3
94.8
59
63
61
Sheet, 0.078" (2.0mm) thick Heat-Treated
at 2050 °F (1121 °C)
Rapid Quenched
Room
400 (204)
600 (316)
800 (427)
51.6
42.0
35.9
32.7
114.9
100.6
98.8
94.3
61
59
68
67
Sheet 0.063 to 0.187" (1.6 to 4.7mm) thick Heat-Treated
at 2050 °F (1121 °C)
Rapid Quenched
400 (204)
600 (316)
800 (427)
1000(538)
42.1
37.7
34.8
33.8
100.8
97.0
95.0
88.9
56
64
65
60
Hastelloy C-276 Equipments
Equipments Specification/Rating
High Pressure Autoclave 50 ml-100 litres, Upto 350 bar, 500°C
Continuous Stirred Tank Reactor 50 ml-100 litres, Upto 350 bar, 500°C
High Pressure Reactors Hydrogenators 50 ml-50000 litres, Upto 150 bar, 500°C
Mini Magnetic Coupling Nano-20, Nano-40, Nano-80
Non-Stirred Pressure Vessels 50 ml-100 litres, Upto 350 bar, 500°C
Catalyst Filters for Precious Metals -
Magnetic Drive -
Other names for Hastelloy® C276
Other names for Hastelloy® C276

 

Alloy C276 Recommended Welding Products
Shielded Metal Arc Welding Gas Tungsten Arc Welding,
Gas Metal Arc Welding
INCO-WELD welding electrode 686CPT INCO-WELD filler metal 686CPT
INCONEL welding electrode C-276 INCONEL filler metal C-276
Hastelloy Alloy C276 Welding Consumables
Welding Electrodes
  • INCONEL welding electrode C-276
  • INCO-WELD welding electrode 686CPT
Fillers
  • INCONEL filler metal C-276
  • INCO-WELD filler metal 686CPT
Find Source Of Good Weldable Hast C276 Material Tested With ASTM G28 Tests
Hast C276 Material Testings
  • Stress Rupture Test
  • Fatigue Test
  • Pitting Corrosion Test
  • Electrochemical Corrosion Test
  • Ultrasonic Testing (UT)
  • Radiographic Testing (RT)
  • Dye Penetrant Testing

 

Nickel C276 Corrosion Rates in Acid Solutions
Solution Temperature Corrosion Rate, mpy (mm/a)
°F °C Alloy C-276 Alloy 22 Alloy 625 Alloy 686
5% H2SO4 + 0.1% HCl Boiling Boiling 22 (0.56) 24 (0.61)
40% H2SO4 + 10% HCl 176 80 26 (0.66) 32 (0.81)
10% H2SO4 Boiling Boiling 20 (0.51) 22 (0.56) 17 (0.43) 3 (0.08)
20% HCl 212 100 154 (3.91) 269 (6.83) 385 (9.78)
5% HCl + 2% HF 158 70 18 (0.46) 40 (1.02) 102 (2.59)
85% H3PO4 Boiling Boiling 10 (0.25) 13 (0.33) >180 (>4.57) 16 (0.41)
10% H2SO4 + 1% HCl Boiling Boiling 70 (1.78) 201 (5.11) 465 (11.68)
10% H2SO4 + 2% HCl Boiling Boiling 138 (3.51) 281 (7.14) 132 (3.35)
10% H2SO4 + 2% HCl 122 50 0.2 (0.005) 0.1 (0.003) 0.1 (0.003) 0 (0)
40% H2SO4 176 80 5 (0.13) 10 (0.25) 5 (0.13)
80% H2SO4 176 80 4 (0.10) 9 (0.23) 6 (0.15) 4 (0.10)
95% H2SO4 122 50 0.1 (0.003) 48 (1.2)
2% HCl Boiling Boiling 43 (1.09) 52 (1.32) 6 (0.15)
5% HCl 140 60 10 (0.25) 46 (1.17) 1.2 (0.30)
10% H2SO4 + 5% HCl Boiling Boiling 256 (6.50) 456 (11.58)
10% HNO3+ 3% HF Boiling Boiling 95 (2.41) 23 (0.61) 28 (0.71)
20% H2SO4 176 80 3 (0.08) 1 (0.03) 1 (0.03)
Hastelloy C276 Types

 

Is UNS N10276 material magnetic? what are its other properties?

It is non-magnetic in both annealed and cold worked conditions.


  • High Tensile & Yield Strengths
  • Impact Resistance
  • Fabricated Easily
  • Versatile
  • Biocompatible and Environment Friendly
  • Non-sparking
Top 7 differences between Hastelloy C276 and C22 Alloy
Property Hastelloy C276 Hastelloy C22
Density (g/cm³) 8.89 8.90
Tensile Strength (MPa) 760 690
Yield Strength (MPa) 290 275
Elongation (%) 40 50
Temperature Range (°C) -196 to 1038 -196 to 1040
Corrosion Resistance Excellent Excellent
C276 Hastelloy Corrosion Resistance in Different Acids
C276 Hastelloy Corrosion Resistance in Different Acids

 

Nickel C276 Corrosion Rates in Various Media
Solution Corrosion Rate Temperature
mpy mm/a °F °C
3% HF 53 1.35 176 80
10% HF 2 0.05 75 24
10% HF 28 0.71 176 80
60% H3PO4 1 0.03 Boiling Boiling
85% H3PO4 <1 <0.03 212 100
20% H3PO4 10 0.25 Boiling Boiling
10% HNO3 15b 0.38b Boiling Boiling
20% H3PO4 <1 <0.03 Boiling Boiling
15% HNO3+ 3% HF 179 4.55 140 60
20% HNO3+ 2% HF 215 5.46 140 60
10% HNO3+ 2% HCl 6.5 0.17 180 82
10% NH3Br 0 0.00 176 80
10% NH3Br 0 0.00 Boiling Boiling
10% HBr <1 <0.03 176 80
10% HBr <1 <0.03 Boiling Boiling
Concentrated HF 1 0.03 75 24
Concentrated HF 34 0.86 176 80
99.9% CH3COOH + 0.1% NaCl <1 <0.03 Boiling Boiling
50% NaOH 1 0.03 Boiling Boiling
Hastelloy® C-276 Corrosion Data
Conc. Wt.% Boiling 50°F 75°F 100°F 125°F 150°F 175°F 200°F 225°F
10°C 24°C 38°C 52°C 66°C 79°C 93°C 107°C
10 - - - - - 0.02 0.51 0.89 -
25 - - - 0.11 0.20 0.29 0.45 0.75 -
30 - - - 0.12 0.20 0.28 0.44 0.75 -
2.5 0.13 - - - - - - - -
15 - - - - 0.01 0.34 0.57 - -
20 - - - <0.01 0.25 0.37 0.51 - -
5 0.78 - - - - - 0.01 0.15 -
7.5 - - - - - 0.01 0.14 0.73 -
40 - - - 0.08 0.13 0.21 0.30 0.53 -
UNS N10276 Corrosion Resistance of Welds
Environment Weld Filler Metal Base Metal Alloy (5-6 mm thickness) Maximum Pitting Depth of Attack, mm Average Results for Duplicate Specimens
GTAW Process GMAW Pulsed Process
Base Metal Weld Metal Base Metal Weld Metal
ASTM G48C INCONEL filler metal C-276 INCONEL alloy C-276 0 0 0 0
INCO-WELD filler metal 686CPT INCONEL alloy C-276 0 0 0 0
Green Death* INCONEL filler metal C-276 INCONEL alloy C-276 0 6.2 0 3.4
INCO-WELD filler metal 686CPT INCONEL alloy C-276 0 0 0 0
Corrosion Resistance of Weldments in Alloy C-276
Environment Weld Filler Metal Base Metal Alloy (5-6 mm thickness) Maximum Pitting Depth of Attack, mm
Average Results for Duplicate Specimens
GTAW Process GMAW Pulsed Process
Base Metal Weld Metal Base Metal Weld Metal
ASTM G48C INCONEL filler metal C-276 INCONEL alloy C-276 0 0 0 0
INCO-WELD filler metal 686CPT INCONEL alloy C-276 0 0 0 0
Green Death* INCONEL filler metal C-276 INCONEL alloy C-276 0 6.2 0 3.4
INCO-WELD filler metal 686CPT INCONEL alloy C-276 0 0 0 0
Average Dynamic Modulus of Elasticity of Werkstoff NR. 2.4819
Form Condition Average Dynamic Modulus of Elasticity,10(6) psi (GPa) Test Temp, °F(°C)
Plate Heat-treated at 2050 °F (1121 °C), Rapid Quenched 29.8 (205) Room
28.3 (195) 400 (204)
27.3 (188) 600 (316)
26.4 (182) 800 (427)
25.5 (176) 1000 (538)
Different Products of Hastelloy C276 Material

Get in touch

Call

+91-22-6639 4858

close