India's Largest Stockist and Supplier Of Nickel Alloys Since 2007

Inconel

Inconel Quick Details
Density 8.2 to 8.3 g/cm³
Melting Point 1,260°C to 1,390°C
Temperature 2000°F (1095°C)
Origin European, Japanese, American, Korean
Inconel Grades Inconel 600, Inconel 625, Inconel 718, Inconel 725
Delivery Time
  • Malaysia : 6-8 Days
  • Italy: 25-30 Days

To Get Quote Within 4 Hours Click Here

 

Inconel Specification

 

Refer Inconel Chemical Composition and Price Per Kg

Inconel Chemical Composition
Inconel Element, proportion by mass (%)
Ni Cr Fe Mo Nb & Ta Co Mn Cu Al Ti Si C S P B
600 ≥72.0 14.0-17.0 6.0-10.0 - - ≤1.0 ≤0.5 - - ≤0.5 ≤0.15 ≤0.015 - -
625 ≥58.0 20.0-23.0 ≤5.0 8.0-10.0 3.15-4.15 ≤1.0 ≤0.5 - ≤0.4 ≤0.4 ≤0.5 ≤0.1 ≤0.015 ≤0.015 -
690 ≥58 27-31 7-11 - - - ≤0.50 ≤0.50 - - ≤0.50 ≤0.05 ≤0.015 - -
617 44.2-61.0 20.0-24.0 ≤3.0 8.0-10.0 - 10.0-15.0 ≤0.5 ≤0.5 0.8-1.5 ≤0.6 ≤0.5 0.05-0.15 ≤0.015 ≤0.015 ≤0.006
718 50.0-55.0 17.0-21.0 Balance 2.8-3.3 4.75-5.5 ≤1.0 ≤0.35 ≤0.3 0.2-0.8 0.65-1.15 ≤0.35 ≤0.08 ≤0.015 ≤0.015 ≤0.006
X-750 ≥70.0 14.0-17.0 5.0-9.0 - 0.7-1.2 ≤1.0 ≤1.0 ≤0.5 0.4-1.0 2.25-2.75 ≤0.5 ≤0.08 ≤0.01 -  
How much does Inconel cost per kg in India?
For Most Updated Inconel Price Click Here
Material Price In INR Price In USD
Inconel Alloy 601 ₹ 5000 - Per kg $ 62.5- Per kg
Inconel Alloy 600 ₹ 4000 - Per kg $ 50- Per kg
Inconel Alloy 625 ₹ 4500 - Per kg $ 56.25 - Per kg
Inconel Alloy 718 ₹ 9000 - Per kg $ 112.5 - Per kg

 

Table of Content
Inconel Specification

Inconel Material Supplier in India in Various Grades

What are the various Inconel Material grades?
Grades UNS/WNR
INCONEL® Alloy 600 UNS N06600/W.Nr. 2.4816
INCONEL® Alloy 601 UNS N06601/W.Nr. 2.4851
INCONEL® Alloy 617 UNS N06617/W.Nr. 2.4663a
INCONEL® Alloy 625 UNS N06625/W.Nr. 2.4856
INCONEL® Alloy 686 UNS N06686/W.Nr. 2.4606
INCONEL® Alloy 690 UNS N06690/W. Nr. 2.4642
INCONEL® Alloy 693 UNS N06693
INCONEL® Alloy 718 UNS N07718/W.Nr. 2.4668
INCONEL® Alloy 725 UNS N07725
INCONEL® Alloy 740H UNS N07740
INCONEL® Alloy X-750 UNS N07750/W. Nr. 2.4669
INCONEL® Alloy 751 UNS N07751
INCONEL® Alloy 783 UNS R30783
Inconel Superalloy AMS Number
AMS Number UNS
AMS 5581 N06625
AMS 5589 N07718
AMS 5590 N07718
AMS 5599 N06625
N06625
N06625
AMS 5715 N06601
N06601
N06601
AMS 5832 N07718
AMS 5869 N06625
N06625
N06625
AMS 5870 N06601
N06601
N06601

Supply Inconel Flat and Rolled Products in Custom Shapes, Refer Properties

Inconel Material Types

 

Inconel Alloy Solid and Liquid Properties
Alloy Liquidus °C (°F) Solidus °C (°F)
Inconel 617 1377 (2,511) 1332 (2,430)
Inconel 625 1350 (2,460) 1290 (2,350)
Inconel 690 1377 (2,511) 1343 (2,449)
Inconel 600 1413 (2,575) 1354 (2,469)
Inconel 718 1336 (2,437) 1260 (2,300)
Inconel X-750 1430 (2,610) 1390 (2,530)
Inconel Alloy Heat Treatment
Inconel Alloy 625
  • High Solution Anneal - 2000/2200°F (1093/1204°C)
  • Low Solution Anneal - 1700/1900°F (927/1038°C)
  • Stress Relieve - 1650°F (899°C), air quench.
Welding Consumables for Inconel
Grades Welding Electrodes Fillers
INCONEL 625 INCONEL 112
  • INCONEL filler metal 625
  • INCOLOY 82
INCONEL 601 INCONEL 117
  • INCONEL filler metal 82
  • INCONEL filler metal 601
  • INCONEL filler metal 617
INCONEL 600 INCONEL 182
  • INCONEL Filler Metal 82
  • INCOFLUX 4
INCONEL X750 -
  • INCONEL Filler Metal 718
INCONEL 725 -
  • INCO-WELD® Filler
  • Metal 725NDUR®
INCONEL 617 INCONEL Welding Electrode 117
  • INCONEL Filler Metal 617
Inconel Temperature Limits
Inconel Alloy 625 Heat Capacity
  • Metric: 0.41 J/g-°C
  • English: 0.098 BTU/lb-°F
Inconel Alloy 600 Heat Capacity
  • Metric: 0.444 J/g-°C
  • English: 0.106 BTU/lb-°F
Buy Inconel Metal Long and Forged Products for Harsh Environments, Refer More Applications
Inconel Metal Applications
Inconel Metal Applications

 

Understand Difference Between Inconel and Monel
What Distinguishes Inconel and Monel?
Properties Inconel Monel
Base Metal Nickel-Chromium Nickel-Copper
Temperature Resistance Up to 1,000°C (1,832°F) or higher Up to 550°C (1,022°F)
Tensile Strength 620 MPa (90,000 psi) for Inconel 718 485 MPa (70,000 psi) for Monel 400
Yield Strength 1,240 MPa (180,000 psi) for Inconel 718 235 MPa (34,000 psi) for Monel 400
Melting Point 1,300-1,400°C (2,372-2,552°F) 1,300°C (2,372°F)
Common Inconel Alloy Trade Names
Grades Alternative Trade Names
Inconel 600® Nickelvac® 600, Ferrochronin® 600
Inconel 617® Nicrofer® 617
Inconel 625® Chornin® 625, Altemp® 625, Nickelvac® 625, Haynes® 625 Nicrofer® 6020
Inconel X750® Haynes X750®, Pyromet® X750, Nickelvac®X750, Nicorros® 7016
Incoloy 800® Ferrochronin® 800, Nickelvac® 800, Nicrofer® 3220
Inconel 718® Nicrofer® 5219, Alvac® 718, Haynes® 718, Altemp® 718
Inconel 601® Pyromet® 601, Nicrofer® 601
Incoloy 825® Nickelvac® 825, Nicrofer 4241®
Characteristics of Inconel Alloys
Characteristics of Inconel Alloys

 

Inconel Material Equivalent
Grades UNS WERKSTOFF NR. JIS BS EN AFNOR GOST
Inconel 601 N06601 2.4851 NCF 601 NA 49 NiCr23Fe NC23FeA XH60BT
Inconel 600 N06600 2.4816 NCF 600 NA 13 NiCr15Fe NC15FE11M МНЖМц 28-2,5-1,5
Inconel 625 N06625 2.4856 NCF 625 NA 21 NiCr22Mo9Nb NC22DNB4M ХН75МБТЮ
Inconel Metal Mechanical Properties
- Inconel 600 Inconel 601 Inconel 625 Inconel 718
Yield strength - Mpa 240min. 300min. 345min. 550 min.
Density 8.4 g/cm³ 8.1g/cm³ 8.4 g/cm³ 8.2 g/cm³
Tensile strength - Mpa 550min. 650min. 760min. 965min
Brinell hardness (HB) ≤195 ≤220 ≤220 ≤363
Elongation % 30min. 30 min. 30 min. 30 min.
Melting Range,℃ 1370-1425 ℃ 1320-1370℃ 1290-1350℃ 1260-1340 ℃
Inconel Alloy Physical Properties
Property Inconel 601 Inconel 600 Inconel 625
Thermal Conductivity 11.0 W/m·K (7.55 BTU/h·ft·°F) 11.4 W/m·K (7.91 BTU/h·ft·°F) 9.0 W/m·K (6.2 BTU/h·ft·°F)
Specific Heat 0.43 J/g·K (0.103 BTU/lb·°F) 0.43 J/g·K (0.103 BTU/lb·°F) 0.42 J/g·K (0.100 BTU/lb·°F)
Electrical Resistivity 1.09 µΩ·cm 1.07 µΩ·cm 1.10 µΩ·cm
Density 8.47 g/cm³ 8.89 g/cm³ 8.44 g/cm³
Melting Point 1370 - 1425°C (2500 - 2600°F) 1370 - 1425°C (2500 - 2600°F) 1290 - 1350°C (2350 - 2460°F)
Modulus of Elasticity 210 GPa (30,500 ksi) 200 GPa (29,000 ksi) 210 GPa (30,500 ksi)
Inconel Metal Melting Point
Inconel Alloy 600
  • Metric: 1354 - 1413 °C
  • English: 2470 - 2580 °F
Inconel Alloy 625
  • 2350 - 2460°F (1280 - 1350°C)
Inconel Alloy 718
  • Solution Treated: 2500-2600°F
  • Solution Treated and Aged: 1370-1430°C
Inconel Material Electrical Conductivity
Material Resistivity Conductivity
- (Ohm-m) (% IACS) (Siemens/m)
Inconel 600 1.014E-06 1.70 9.860E+05
Inconel 601 1.190E-06 1.45 -
Inconel 617 1.220E-06 1.41 -
Inconel 625 1.290E-06 1.34 -
Inconel 600 1.030E-06 1.67 -
Inconel 690 1.480E-07 11.65 -
Inconel 718 1.250E-06 1.38 -
Inconel X750 1.220E-06 1.41 -
Inconel Superalloy Hardness
Material Grade Hardness HB
Inconel Tube 625 Seamless and Welded -
Inconel Round Bar 600 65-85B
Inconel 625 Round Bar 625 ≤ 287 HB
Inconel 625 Plate 625 145-240
Inconel Plate 600 65-85B
Inconel Pipe 600 88B max
Inconel Wire 600 -
Shipping Time As Per Location
Changes in Price Extra 5 %
Export to Shipping Time in Days
Switzerland 45-60
Slovakia 45-60
Hungary 45
Slovenia 60
Malta  60
Czech Republic 45
Albania  45
Austria 60
Finland 45-60
Ireland 60
Croatia 60
Portugal 45
Singapore  8
Malaysia  7
Indonesia  7

Get in touch

Call

+91-22-6639 4858

close